S65.10-4576-09
1 | Expose spot welds on side roof paneling (1) and cut out (areas A and B). |
Cut out spot welds through two sheet metal thicknesses (arrows). |
2 | Heat side roof paneling (1) in crosshatched areas. |
Crosshatched areas are bonded with adhesive. |
3 | Remove damaged side roof paneling (1). |
4 | Grind mating surfaces down to bare metal in crosshatched areas and around holes. |
Sand down spot weld flanges to bare metal on both sides. |
5 | Remove shavings and drill chips. |
6 | Coat insides of spot weld flanges with zinc dust paint. |
Do not coat bonding surface (area C) with zinc dust paint. |
Observe pretreatment of bonding surface (area C). |
S65.10-4577-06