S63.20-4680-09
a | Dimension approx. 200 mm |
1 | Mark separating point and cut (area A). |
Do not cut too deeply. |
2 | Expose spot welds on partial inner upper A-pillar reinforcement (1) and cut (areas B and C). |
3 | Heat partial inner upper A-pillar reinforcement (1) in crosshatched areas. |
Crosshatched areas are bonded with adhesive. |
4 | Remove damaged partial inner upper A-pillar reinforcement (1). |
S63.20-4681-06
S63.20-4682-09
5 | Drill holes for MAG welding (area D). |
6 | Grind mating surfaces down to bare metal in crosshatched areas and around the holes (area D). |
Sand down spot weld flanges to bare metal on both sides. |
7 | Remove shavings and drill chips. |
8 | Coat insides of spot weld flanges with zinc dust paint. |
Do not coat bonding surfaces with zinc dust paint (areas E and F). |
Observe pretreatment of bonding surfaces (areas E and F). |