S63.10-6183-09
x | Dimension approx. 15 mm |
1 | Mark separating point on side wall paneling (1) and cut (area A). |
Do not cut too deeply. |
2 | Expose spot welds on side wall paneling (1) and cut out (area D). |
3 | Expose spot weld and drill through (area E). |
S63.10-6184-06
S63.10-6185-09
4 | Expose spot welds on side wall paneling (1) and cut out (areas F bis H). |
Cut out spot welds (arrows) through two panel thicknesses. |
5 | Expose laser weld seams on side wall paneling (1) and cut (areas I and J). |
S63.10-6186-09
6 | Expose spot welds on bottom section of rear side wall paneling (2) and cut out (areas K to N). |
7 | Expose MAG spot welds on rear side wall paneling bottom section (2) and cut out (area O). |
8 | Cut inert gas welds on rear side wall paneling bottom section (2 (area P). |
9 | Heat sidewall paneling (1) in crosshatched areas. |
Cross-hatched areas are bonded. |
10 | Remove damaged side wall paneling (1). |
S63.10-6187-06
11 | Grind mating surfaces down to bare metal in crosshatched areas and around hole (area Q). |
Sand down spot weld flanges to bare metal on both sides. |
12 | Remove shavings and drill chips. |
13 | Coat insides of spot weld flanges with zinc dust paint. |
S63.10-6188-06
14 | Grind mating surfaces down to bare metal in crosshatched areas and around hole (area R). |
Sand down spot weld flanges to bare metal on both sides. |
15 | Remove shavings and drill chips. |
16 | Coat insides of spot weld flanges with zinc dust paint. |
S63.10-6189-06