P63.30-2412-06
1 Scribe cut along broken line in area E on longitudinal member inner shell (1) according to old part removed.
2 Cut along broken line in area E on longitudinal member inner shell (1).
3 Grind mating surface down to bare metal in area D on front longitudinal member inner shell section (1.1) on one side.
4 Grind mating surface down to bare metal in area B on front longitudinal member inner shell section (1.1) on one side.
5 Grind mating surface down to bare metal in area C on front longitudinal member inner shell section (1.1) on both sides.
6 Grind mating surface down to bare metal in area A on front longitudinal member inner shell section (1.1) on both sides. Coat insides of spot weld flanges with zinc dust paint.