P98.00-0867-74
P98.00-0868-71
P98.00-0869-71
Description | Cause | Remedy |
Paintwork does not have a smooth surface. Structure similar to orange peel. | Wrong spraying technique. Viscosity too high. Spraying pressure too high/too low. Spray gun interval too great. Spray nozzle too large. Air drying time not maintained. Processing temperature too high. Nominal layer thickness not maintained. | A slight orange peel effect is permissible, heavy orange peel effect is not permissible Sand with P 1500 followed by P 2000 grain sand paper and polish paint surface mechanically with Mercedes-Benz Paint Cleaner. Repainting is required only in extreme cases. |